• Original article •
WANG Han,LAN Heqing,GENG Keming, LV Shiping, FANG Xu
Published:
Abstract: Six kinds of Cr2O3-Al2O3 fused grains (the mass percent of Cr2O3 was 15%, 40%, 50%, 60%, 85% and 99%, respectively) were prepared-using chrome green and Al2O3 powder as starting materials by electrofusion, named as CR15, CR40, CR50, CR60, CR85, and CR99, respectively. The corrosion resistance of the six kinds of Cr2O3-Al2O3 fused grains (4-1 mm) was studied using rotary slag corrosion method. The results show that: (1)the corrosion resistance of the fused grains increases with the Cr2O3 content and the grain size increasing; (2)the grains of CR99 and CR85 with higher Cr2O3 content are corroded at the slag surface layer, because FeO and Al2O3 in the slag corrode the grains; FeO reacts with Cr2O3 in the aggregates forming (Fe, Cr)3O4 spinel firstly, and the spinel reacts with other phases forming composite spinel; when FeO is fully consumed, Al2O3 penetrated into the grains reacts with Cr2O3 forming Al2O3-Cr2O3 solid solution on the grains surface; (3) for CR60, the corrosion exists both in the slag surface layer and in the penetration layer; in the penetration layer, CaO and SiO2 react with Al2O3 in Al2O3-Cr2O3 solid solution forming anorthite, gehlenite, and glass phase; the grains of CR50, CR40 and CR15 have the same corrosion mechanism with CR60 in the penetration layer.
Key words: high chrome refractories, chrome oxide-alumina fused grains, rotary slag corrosion method, corrosion mechanism
WANG Han,LAN Heqing,GENG Keming, LV Shiping, FANG Xu. Corrosion Resistance of Fused Cr2O3-Al2O3 Grains with Different Compositions[J]. China's Refractories.
/ Recommend
Add to citation manager EndNote|Ris|BibTeX
URL: http://www.cnref.cn/EN/
http://www.cnref.cn/EN/Y2012/V21/I2/